Caution
① Proper preheating(50~150℃/122~302℉) and interpass temperature are required in order to release hydrogen which may cause cracking in weld metal when wires are used for medium and heavy plates.
② High-voltage or high-speed for one-side welding might cause hot cracking on the root bead.