Caution
① Dry the electrodes at 350~400℃(662~752℉) for 60 minutes before use.
② Adopt back step method or strike the arc on a small steel plate prepared for this particular purpose because arc striking on the base metal is in danger of initiating cracking.
③ Keep the arc as short as possible. "
Purpose
① High tensile weathering steel
Attribute
① Suitable for off- and on-shore construction
② High resistance to corrosion caused by seawater or combinations of oil, gas and seawater
③ Contains Cu, Ni and Cr (All-weld metal)
S-7018.W
Теплоустойчивые сталиS-7018.W
Type
Basic
Industry
Heavy Equipment|Offshore structures|Energy & Power Plants|Steel Fabric
Caution
① Dry the electrodes at 350~400℃(662~752℉) for 60 minutes before use.
② Adopt back step method or strike the arc on a small steel plate prepared for this particular purpose because arc striking on the base metal is in danger of initiating cracking.
③ Preheat at 80~100℃(176~212℉)before use. The temperature to be applied varies in accordance with plate thickness and steel kind.
Purpose
① High tensile weathering steel
Attribute
① Suitable for off- and on-shore construction
② High resistance to corrosion caused by seawater or combinations of oil, gas and seawater
③ Contains Cu, Ni and Cr (All-weld metal)