HYUNDAI WELDING

事業紹介

ALL PRODUCT

サブマージアーク溶接材料

S-460Y x H-14

S-460Y S-460Y x H-14

Type
Industry
JIS Z3183 S584-H
EN ISO 14174 S A FB 1 / 14171 S4
KS B0531 S584-H
AWS A5.23/ASME SFA5.23 F8A8-EH14-G
  • Caution ① Dry at 300~350℃(572~662℉) for 60 minutes before use.

    ② Use welding current and speed as low as possible at the first layer of groove to avoid cracking.

    ③ If weld heat input is managed below 30KJ/cm, a better impact toughness can be achieved.

    ④ When restraint stress is high or welding a thick plate, preheat according to rules.
  • Purpose ① Shipbuilding

    ② High strength steels (EH47)
  • Attribute ① Good impact value at low temperature and high tensile strength

    ② Single and multi electrode welding applicable

    ③ Density : 1.2g/cm3
top